The effect of different surface treatments on the shear bond strength of luting cements to titanium.

PubWeight™: 0.77‹?›

🔗 View Article (PMID 23217469)

Published in J Prosthet Dent on December 01, 2012

Authors

Filipe de Oliveira Abi-Rached1, Renata Garcia Fonseca, Isabella Gagliardi Haneda, Antonio Alves de Almeida-Júnior, Gelson Luis Adabo

Author Affiliations

1: Department of Dental Materials and Prosthodontics, Araraquara Dental School, São Paulo State University (UNESP), Araraquara, São Paulo, Brazil.

Articles by these authors

Shear bond strength of metal-ceramic repair systems. J Prosthet Dent (2006) 0.97

Effect of metal primers on bond strength of resin cements to base metals. J Prosthet Dent (2009) 0.91

The volumetric fraction of inorganic particles and the flexural strength of composites for posterior teeth. J Dent (2003) 0.86

Compressive strength and compressive fatigue limit of conventional and high viscosity posterior resin composites. Braz Oral Res (2006) 0.84

Diametral tensile strength of dual-curing resin cements submitted exclusively to autopolymerization. Quintessence Int (2007) 0.81

The influence of chemical activation on hardness of dual-curing resin cements. Braz Oral Res (2004) 0.80

Vickers hardness of cast commercially pure titanium and Ti-6Al-4V alloy submitted to heat treatments. Braz Dent J (2006) 0.79

Shear bond strength of metal-ceramic repair systems. Gen Dent (2009) 0.79

Influence of activation modes on diametral tensile strength of dual-curing resin cements. Braz Oral Res (2006) 0.79

Influence of microwave sterilization on the cutting capacity of carbide burs. J Appl Oral Sci (2009) 0.79

Efficacy of air-abrasion technique and additional surface treatment at titanium/resin cement interface. J Adhes Dent (2012) 0.79

Internal adaptation of cast titanium crowns. J Appl Oral Sci (2007) 0.79

Effect of cyclic compressive loading on the bond strength of an adhesive system to dentin after collagen removal. J Adhes Dent (2005) 0.78

The influence of short-heating-cycle investments on the quality of commercially pure titanium castings. J Prosthet Dent (2010) 0.77

Effect of surface treatments on the bond strength of a resin cement to commercially pure titanium. Braz Dent J (2010) 0.76

Influence of the final temperature of investment healting on the tensile strength and Vickers hardness of CP Ti and Ti-6Al-4V alloy. J Appl Oral Sci (2007) 0.75

Clinical fractures of veneered zirconia single crowns. Gen Dent (2013) 0.75

Evaluation of the thermal shrinkage of titanium and the setting and thermal expansion of phosphate-bonded investments. J Prosthet Dent (2007) 0.75

The effect of mold temperature on castability of CP Ti and Ti-6Al-4V castings into phosphate bonded investment materials. Dent Mater (2006) 0.75

Efficacy of surface treatments on the bond strength of resin cements to two brands of zirconia ceramic. J Adhes Dent (2013) 0.75

Improvement to the marginal coping fit of commercially pure titanium cast in phosphate-bonded investment by using a simple pattern coating technique. J Prosthet Dent (2012) 0.75

The effect of coating patterns with spinel-based investment on the castability and porosity of titanium cast into three phosphate-bonded investments. J Prosthodont (2010) 0.75

Effect of thermal treatments on tensile strength of commercially cast pure titanium and Ti-6Al-4V alloys. J Mater Sci Mater Med (2005) 0.75

Shear bond strength of different repair systems to titanium after water aging. Oper Dent (2012) 0.75

Effect of phosphate-bonded investments on titanium reaction layer and crown fit. Braz Oral Res (2010) 0.75

Effect of surface and heat treatments on the biaxial flexural strength and phase transformation of a Y-TZP ceramic. J Adhes Dent (2014) 0.75

Effect of metal conditioners on the adhesive bonding of resin cements to cast titanium. Quintessence Int (2007) 0.75